Degussa Frit 90205

Alternate Names: 90205 Bleiborsilikat

Description: Bleibo-silikat

Oxide Analysis Formula Tolerance
ZnO 16.04% 0.45
PbO 53.76% 0.55
SiO2 21.06% 0.80
B2O3 9.14% 0.30
Oxide Weight 228.36
Formula Weight 228.36

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.