Degussa Frit 90187

Description: Bienatriumbor-silikat

Oxide Analysis Formula Tolerance
SiO2 29.82% 1.50
B2O3 23.02% 1.00
Na2O 10.25% 0.50
PbO 36.91% 0.50
Oxide Weight 302.40
Formula Weight 302.40

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 94 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 499C
Heating Microscope Analysis for Frits 590C
Heating Microscope Analysis for Frits 680C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy