Oxide Analysis Formula Tolerance
Na2O 16.25% 1.00
B2O3 36.49% 2.00
SiO2 47.26% 3.00
Oxide Weight 381.54
Formula Weight 381.54

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 85 X 10-7 (20-400C)
Heating Microscope Analysis for Frits 514C
Heating Microscope Analysis for Frits 685C
Heating Microscope Analysis for Frits 780C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy