Degussa Frit 90142

Alternate Names: 90142 Calziumboratfritte

Description: Calziumborat-fritte

Oxide Analysis Formula Tolerance
CaO 25.71% 1.00
SiO2 33.05% 1.20
B2O3 31.89% 1.00
Al2O3 9.35% 0.20
Oxide Weight 218.20
Formula Weight 218.20

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 66 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 632C
Heating Microscope Analysis for Frits 900C
Heating Microscope Analysis for Frits 960C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy