Degussa Frit 90062

Alternate Names: 90062 Bleiborsilikat

Description: Bleiborsilikat

Oxide Analysis Formula Tolerance
PbO 62.41% 1.00
SiO2 8.40% 0.50
B2O3 29.19% 1.50
Oxide Weight 357.63
Formula Weight 357.63

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 79 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 440C
Heating Microscope Analysis for Frits 550C
Heating Microscope Analysis for Frits 640C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy