Degussa Frit 90001

Alternate Names: 90001 Bleisilikat

Description: Bleisilikat

Oxide Analysis Formula Tolerance
PbO 78.79% 1.00
SiO2 21.21% 1.00
Oxide Weight 283.28
Formula Weight 283.28

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 96 x 10-7 (20-400C)
Heating Microscope Analysis for Frits 410C
Heating Microscope Analysis for Frits 530C
Heating Microscope Analysis for Frits 695C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy