| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| AlF3 | 29.80% | 1.00 | |
| NaF | 44.80% | 3.00 | |
| CaF2 | 25.40% | 0.92 | |
| Oxide Weight | 281.54 | ||
| Formula Weight | 281.54 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 905C |
|---|
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |