Chamotte

Description: Calcined fireclay

Notes

A light colored refractory grog or a the waste products of ceramic granites and sanitaryware. Often used as a filler in tile manufacture and even slipcast products. It is used in Europe.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Fireclay
Typecodes Aggregate
Granular materials intended to impart raw and fired structural strength or thermal expansion properties to bodies or deliver special speckling effects in glazes.
URLs https://www.imerys.com/product-ranges/chamotte-ceramics
Chamotte information from Imerys
Chamotte—also known as 'grog', 'firesand' or “fireclay”—is calcined clay containing a high proportion of alumina. It is produced by firing selected fire clays in a rotary kiln.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy