Ceradel Frit C 1254

Alternate Names: Fritte C1254, Fritte C 1254, Ceradel Frit 1254

Description: Fritte calco-alcaline sans plomb

Oxide Analysis Formula Tolerance
Al2O3 7.38% 0.20
B2O3 27.73% 1.10
Na2O 11.22% 0.50
CaO 10.15% 0.50
SiO2 43.51% 2.00
Oxide Weight 276.30
Formula Weight 276.30

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 72x10-7 (20/300C)
Frit Softening Point 800-920C