1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Calcium and Sodium Aluminum Silicate Eutectic

Oxide Analysis Formula Tolerance
Na2O 15.60% 0.71
CaO 5.80% 0.29
Al2O3 36.00% 0.99
SiO2 42.60% 2.00
Oxide Weight 281.69
Formula Weight 281.69

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1130C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.