Cadmium Oxide

Formula: CdO

Oxide Analysis Formula Tolerance
CdO 100.00% 1.00
Oxide Weight 128.41
Formula Weight 128.41

Notes

Cadmium oxide is insoluble in water and alkalis, but soluble in acids and ammonium salts.

See notes for CdO oxide for information about participation in glaze chemistry.

Related Information

Links

Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
URLs http://en.wikipedia.org/wiki/Cadmium_oxide
Cadmium oxide on Wikipedia
Materials Stains Encapsulated
Oxides CdO - Cadmium Oxide
Glossary Encapsulated Stain
This is a type of stain manufacture that enables the use of metal oxides (like cadmium) under temperature conditions in which they would normally fail.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy