1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

C-90 Magnesite

Oxide Analysis Formula Tolerance
CaO 1.50% 1.72
MgO 91.60% 145.81
Al2O3 1.59% 1.00
SiO2 4.00% 4.27
Fe2O3 0.81% 0.32
LOI 0.50%n/a
Oxide Weight 6,383.02
Formula Weight 6,415.09