Burgess Iceberg Calcined Kaolin

Alternate Names: Icecap K

Oxide Analysis Formula Tolerance
SiO2 51.70% 2.03 0.7
Al2O3 43.20% 1.00 1.0
Fe2O3 0.20% -
TiO2 2.00% 0.06 0.5
LOI 0.50%n/a
Oxide Weight 229.26
Formula Weight 230.42

Notes

Conventionally calcined kaolin.
Burgess Icecap K, Iceberg and No. 30 calcined kaolins differ slightly in the pH, brightness, #325 residue, % free moisture. None of the differences should have significant effects on ceramic glaze and body applications.
However their Optiwhite thermo optic kaolins have the same chemistry but have an amorphous particle shape and lower specific gravity.

Related Information

Links

Materials Calcined Kaolin
This is kaolin powder that has been fired in a furnace to remove the 12% crystal water and render it non-plastic.
URLs http://burgesspigment.com/BurgessWebsite.nsf/ICEBERG.pdf?OpenFileResource
Iceberg Kaolin Datasheet
URLs https://digitalfire.com/4sight/datasheets/BurgessKaolin.pdf
Burgess Kaolin Data Sheet
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.

Data

GE Brightness 85-92%
% Passing 325 Mesh Wet 99.95+%
Particle Shape (1-7 microns) Thin flat plate
Density (Specific Gravity) 2.63
Moisture Content - Powder 0.25-0.5%
Median Particle Size (Microns) 1.4 microns
pH for dry powder 5.5

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy