1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Bristol Silica

Oxide Analysis Formula Tolerance
CaO 0.45% 2.10
Al2O3 0.39% 1.00
P2O5 0.35% 0.65
SiO2 98.71% 429.56
Fe2O3 0.10% 0.16
Oxide Weight 26,153.85
Formula Weight 26,153.85

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.