Description: Dilute solution of sodium hypochlorite

Notes

Common laundry bleach (tradenamed "Clorox" in the US, "Javex" in Canada) is a solution of 5.75% sodium hypochlorite, NaOCl. On heating the composition reverts to lye (NaOH) and liberates chlorine gas and some nascent oxygen.

It is an effective against fungi, bacteria, algae and mildew agent at concentrations above 10 ppm.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Biocide
These are added to glazes and bodies to prevent the growth of micro organisms. Often targeted at bacteria, mold or fungi.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy