Bentolite B

Alternate Names: Bentolite BC

Description: White burning processed bentonite

Oxide Analysis Formula Tolerance
SiO2 62.90% 9.88
MgO 2.40% 0.56
Al2O3 17.10% 1.58
Fe2O3 4.80% 0.28
CaO 0.70% 0.12
Na2O 2.10% 0.32
TiO2 0.10% 0.01
LOI 9.50%n/a
Oxide Weight 850.79
Formula Weight 940.10

Notes

A high purity montmorillonite refined to meet the thixotropic needs of water-based systems where high viscosity is required without the demand for whiteness (it has a much higher iron content that the other bentonlite products). Mineral Colloid® BP provides suspension stability and viscosity control. It is targetted at the Home Care and Personal Care markets.

Was made by Southern Clay products but discontinued by new owners.

Related Information

Links

Materials Bentolite L-3
Materials Laponite RD
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy