Barium Titanate

Formula: BaTiO3

Notes

Barium titanates (pure BaTiO3 and doped variations) have excellent dielectric properties (they are very good insulators) and are used to make capacitors in the electronics industry. Capacitors have thin conducting metal plates separated by an insulating material (the thinner the insulator the more layers devices can have and the smaller they can be). Recent advances in processing barium titanate powders have made it possible to decrease the dielectric layer to thicknesses approaching two microns.

Related Information

Links

Oxide Analysis Formula Tolerance
Typecodes Non-Oxide Material
Many of these materials are not used in traditional ceramics but they have such incredible properties that some have been included in this database.
Materials Titanium Diboride
Materials Silicon Carbide
Materials Boron Carbide

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy