Andesine

Description: Plagioclase Feldspar

Oxide Analysis Formula Tolerance
CaO 6.99% 0.50
Na2O 7.72% 0.50
Al2O3 25.41% 1.00
SiO2 59.88% 4.00
Oxide Weight 401.42
Formula Weight 401.42

Notes

A plagioclase feldspar. The chemistry given is theoretical, actual materials will vary.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
Minerals Plagioclase
Plagioclase feldspar is not one mineral but a series between two: Albite - NaAlSi₃O₈ (high sodium) a

Data

Hardness (Moh) 6.5
Frit Softening Point 1350C
Density (Specific Gravity) 2.70