Formula: SiO2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 100.00% | 1.00 | |
| Oxide Weight | 60.10 | ||
| Formula Weight | 60.10 | ||
We are not yet aware of the uses of this material in ceramics. Since amorphous silica and regular silica (or quartz) have the same chemistry, then in glazes they should produce the same results (since they both will dissolve into the melt). Likewise, in clay bodies, the first time the material is heated to sufficient temperature it will convert into the preferred crystalline state.
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |