Ammonium Molybdate Tetrahydrate

Formula: (NH4)6Mo7O24.4H2O

Oxide Analysis Formula Tolerance
MoO3 81.55% 1.00
LOI 18.44%n/a
Oxide Weight 143.94
Formula Weight 176.48

Notes

CAS Number: 12054-85-2
Merck Number: 14,533
UN Number: UN3288

Substance is listed in Toxic Substance Control Act (TSCA) inventory.

This decomposes in stages, finally liberating MoO3

Related Information

Links

Hazards Molybdenum Compounds Toxicology
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

Data

Frit Softening Point 190C
Density (Specific Gravity) 2.498

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy