Amical

Description: Kills fungus in clays and glazes

Notes

This is not specifically marketed for ceramics but is used for indirect food applications so it should be OK. But it is specifically for fungus and there are other microbial to consider in ceramics (e.g. bacteria, mold, algae, yeats).

It is EPA-Registered Fungicide for Industrial Products and Process Systems. General AMICAL™ Preservatives are antimicrobial agents, based on the active Diiodomethyl-ptolylsulfone, which are useful for the control of microbial degradation in a variety of end-use applications. They are EPA-registered for use in adhesives, paper coatings, plastics, tanned leather, caulks, metalworking fluids, textiles, coatings and wood preservation.

The advantages of using AMICAL Preservatives are:
• Extremely effective active antifungal agent
• FDA clearances in the U.S. for several indirect food contact applications
• Effective over a broad pH range (2-11)
• Available in easy-to-use liquid or powder forms
• Non dermally-irritating

Related Information

Links

Oxide Analysis Formula Tolerance
URLs http://msdssearch.dow.com/PublishedLiteratureDOWCOM/dh_004a/0901b8038004aa8f.pdf?filepath=biocides/pdfs/noreg/253-01212.pdf&fromPage=GetDoc
Amical Technical Information from Dow Chemical
URLs https://toxnet.nlm.nih.gov/cgi-bin/sis/search/a?dbs+hsdb:@term+@DOCNO+8033
Amical information on Toxnet
URLs https://www.dupont.com/products/amical48.html
Dupont Amical product page
Materials Tektamer 38 Biocide
Typecodes Biocide
These are added to glazes and bodies to prevent the growth of micro organisms. Often targeted at bacteria, mold or fungi.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy