Alternate Names: Ajax P Casting Kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.05% | - | |
| Na2O | 0.30% | 0.01 | |
| MgO | 0.30% | 0.02 | |
| TiO2 | 1.40% | 0.05 | |
| Al2O3 | 38.40% | 1.00 | |
| SiO2 | 45.30% | 2.00 | |
| Fe2O3 | 0.30% | - | |
| LOI | 13.90% | n/a | |
| Oxide Weight | 228.57 | ||
| Formula Weight | 265.47 | ||
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| Pyrometric Cone Equivalent | 36 |
|---|---|
| Dry M.O.R. (50% Silica) | 932C |