Glazes

Notes

Range % Thermal Expan
Opaque Whites: 200-500C
--------------------------------------------------------
9/0501036 Zircon bright white 1080-1180 .320
9/0501020 Bright white 1120-1140 .310
9/0501027 White opaque 1080-1180 .295
9/0501019 White opaque 1040-1150 .305

Unleaded Transparents

9/0500015 Very bright 1050-1180 .337
9/0500048 Bright high temp. 1200-1300 .348
9/0500070 Fast fire hight temp. 1180-1220 .353
9/0500057 Earthenware 1060-1140 .32

Lead Transparents (Low Solubility)

9/0510012 Bright bone china 1000-1100 .352
9/0510023 Bright clear 1080-1140 .366
9/0510004 Bright clear 1020-1120 .308
9/0510015 Bone china glaze 1000-1100 .330

Oxide Analysis Formula Tolerance

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy