| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 19.50% | 1.00 | |
| SiO2 | 63.00% | 3.33 | |
| LOI | 17.50% | n/a | |
| Oxide Weight | 262.31 | ||
| Formula Weight | 317.95 | ||
| Materials |
Glassil A
|