Fused Alumina

Oxide Analysis Formula Tolerance
TiO2 2.84% 0.04
Al2O3 96.99% 1.00
SiO2 0.07% -
Fe2O3 0.09% -
Oxide Weight 105.15
Formula Weight 105.15