Pemco Frit Pb-1307

Alternate Names: Frit Pb1307

Description: High lead zinc containing wall tile frit

Oxide Analysis Formula Tolerance
CaO 5.40% 0.23
Na2O 2.20% 0.09
PbO 39.90% 0.43
ZnO 8.70% 0.26
B2O3 9.20% 0.32
Al2O3 6.30% 0.15
SiO2 28.30% 1.13
Oxide Weight 239.59
Formula Weight 239.59

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.8 x 10-6 (50-450C)
Frit Softening Point 1250F
Frit Melting Range (C) 1250-1300F
I.F.P. (celsius) 547C