Pemco Frit P-4N57

Alternate Names: 4N57,4N-57

Oxide Analysis Formula Tolerance
Li2O 0.30% 0.08
Na2O 6.84% 0.92
B2O3 18.84% 2.25
Al2O3 7.16% 0.58
SiO2 66.87% 9.25
Oxide Weight 831.08
Formula Weight 831.08

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy