Pemco Frit P-2V25

Alternate Names: 2V25,2V-25

Description: Low temperature flux frit used in brick coatings

Oxide Analysis Formula Tolerance
CaO 22.20% 0.55
MgO 3.00% 0.10
Na2O 15.30% 0.34
B2O3 21.50% 0.43
Al2O3 0.70% 0.01
SiO2 25.10% 0.58
F 12.20% 0.90
Oxide Weight 139.48
Formula Weight 139.48

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 4GF45C
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 15.00
Co-efficient of Linear Expansion 15.0 x 10-6 (50-350C)
Frit Softening Point 1250F
Frit Melting Range (C) 1220-1270F
I.F.P. (celsius) 482C