Pemco Frit P-1000

Alternate Names: Frit 1000, Frit P1000

Description: LEADLESS FRIT

Oxide Analysis Formula Tolerance
CaO 14.60% 0.68
Na2O 7.60% 0.32
ZrO2 17.60% 0.37
B2O3 17.00% 0.64
SiO2 45.20% 1.96
Oxide Weight 266.44
Formula Weight 266.44

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.90
Frit Softening Point 1590F