Description: Lead borosilicate glaze frit cone 08-02
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 6.47% | 0.28 | |
| PbO | 59.17% | 0.72 | |
| B2O3 | 14.54% | 0.57 | |
| SiO2 | 19.82% | 0.89 | |
| Oxide Weight | 270.72 | ||
| Formula Weight | 270.72 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3419
|
| Materials |
Hommel Frit 240
|
| Materials |
Frit A 2010
|
| Materials |
Hommel Frit 33
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| By Tony Hansen Follow me on ![]() | ![]() |