Fusion Frit F-77

Alternate Names: Frit F77

Description: BOND FRIT

Oxide Analysis Formula Tolerance
CaO 18.00% 0.61
MgO 4.30% 0.20
Na2O 6.20% 0.19
B2O3 45.00% 1.23
Al2O3 2.50% 0.05
SiO2 24.00% 0.76
Oxide Weight 189.55
Formula Weight 189.55

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-309
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.