Alternate Names: F60 Fusion, Frit F60
Description: Zinc free calcium and sodium frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.50% | 0.36 | |
| Na2O | 15.00% | 0.64 | |
| B2O3 | 21.50% | 0.82 | |
| SiO2 | 56.00% | 2.48 | |
| Oxide Weight | 266.22 | ||
| Formula Weight | 266.22 | ||
| Materials |
Ferro Frit 3278
|
| Materials |
Pemco Frit P-830
|
| Materials |
Hommel Frit K-3
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.76 x 10-6 |
|---|---|
| Frit Softening Point | 1600F |