Pemco Frit P-83

Alternate Names: Frit P83, Frit 83

Description: Medium Lead Frit

Oxide Analysis Formula Tolerance
Na2O 5.07% 0.28
PbO 46.96% 0.72
B2O3 5.29% 0.26
SiO2 42.68% 2.43
Oxide Weight 342.27
Formula Weight 342.27

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Frit HP33
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.