Ferro Frit 3465

Description: Low lead high borax frit cone 08-02

Oxide Analysis Formula Tolerance
CaO 6.50% 0.31
Na2O 14.40% 0.62
PbO 6.40% 0.08
B2O3 20.20% 0.77
SiO2 52.50% 2.32
Oxide Weight 265.40
Formula Weight 265.40

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit Pb-943
Materials Hommel Frit 18
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.70
Frit Melting Range (C) 1600F