Ferro Frit 3379

Description: Lead silicate frit

Oxide Analysis Formula Tolerance
PbO 89.80% 1.00
SiO2 10.20% 0.42
Oxide Weight 248.56
Formula Weight 248.56

Notes

Has more PbO than a lead monosilicate.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.