Ferro Frit 3302-D

Alternate Names: Formerly Frit 1085

Description: Opaque frit for white and pastel glazes cone 04-06

Oxide Analysis Formula Tolerance
CaO 6.00% 0.46
MgO 0.60% 0.06
Na2O 6.00% 0.42
ZnO 1.10% 0.06
ZrO2 12.23% 0.43
B2O3 13.53% 0.84
Al2O3 4.10% 0.17
SiO2 56.45% 4.05
Oxide Weight 431.00
Formula Weight 431.00

Notes

This is supposedly an old name for Frit DA9146

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Potclays Frit 2270
Materials Hommel Frit 698
Materials Ferro Frit 1085
Materials Ferro Frit 9102
Materials Ferro Frit 9146
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.