Ferro Frit 4171

Alternate Names: Frit 1057, Frit 3271, Frit DA4171

Description: Leadless calcium borosilicate frit (was Frit 3271, Frit 1057)

Oxide Analysis Formula Tolerance
CaO 11.00% 0.49
Na2O 12.80% 0.51
B2O3 21.60% 0.77
SiO2 54.60% 2.26
Oxide Weight 248.43
Formula Weight 248.43

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 49
Materials Glostex Frit H-2
Materials Ferro Frit 1057
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.30
Frit Softening Point 558C
Frit Melting Range (C) 1040-1100C
Glass Transition Temperature 590C