Ferro Frit 3264

Description: Leadless high sodium borosilicate

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
MgO 0.10% 0.01
Na2O 20.90% 0.99
B2O3 21.10% 0.89
Al2O3 6.70% 0.19
SiO2 51.10% 2.49
Oxide Weight 292.95
Formula Weight 292.95

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Fusion Frit F-499
Materials Hommel Frit 5
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 11.0 x 10-6 (50-450C)
Frit Melting Range (C) 1400F
By Tony Hansen