Ferro Frit 3191

Alternate Names: F3191

Description: A source of alkali borate for use in abrasives industry

Oxide Analysis Formula Tolerance
CaO 11.27% 0.50
Na2O 12.46% 0.50
B2O3 27.97% 1.00
SiO2 48.30% 2.00
Oxide Weight 248.84
Formula Weight 248.84

Related Information

Links

Materials Fusion Frit F-34
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.2 x 10-6 (50-450C)
Frit Melting Range (C) 1300F