Fabi Talc 1656

Oxide Analysis Formula Tolerance
SiO2 61.50% 1.32
MgO 31.00% 0.99
CaO 0.40% 0.01
Fe2O3 0.60% -
Al2O3 0.50% 0.01
Oxide Weight 121.08
Formula Weight 121.08

Related Information

FabiTalc Technical Data Sheet


Click here view full document

FabiTalc SDS


Click here view full document

Links

URLs https://www.imifabi.com/
IMIFABI Talc home page
A leading global talc manufacturer. Established in the 1950's, in Valmalenco (SO) Italy. IMIFABI's operating network produces high quality talc products for customers in plastic, paper, paints and fillers, animal feed, building coatings, ceramics, pharmaceuticals and more. The company claims commitment to sustainable value creation.