General Frit GF-43

Description: High lead boron frit

Oxide Analysis Formula Tolerance
Na2O 0.30% 0.02
PbO 42.40% 0.98
Al2O3 5.80% 0.29
B2O3 10.20% 0.75
SiO2 41.40% 3.54
Oxide Weight 513.85
Formula Weight 513.85

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.