37080 Alkaliborsilikaat

Oxide Analysis Formula Tolerance
CaO 1.56% 0.10
MgO 2.24% 0.20
Na2O 12.07% 0.70
Al2O3 5.67% 0.20
B2O3 11.61% 0.60
SiO2 66.85% 4.00
Oxide Weight 359.62
Formula Weight 359.62