1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fillite

Oxide Analysis Formula Tolerance
Al2O3 30.00% 1.00 3
SiO2 60.00% 3.39 5
Fe2O3 3.00% 0.06 1
Oxide Weight 316.20
Formula Weight 316.20

Notes

Fillite "cenospheres" are lightweight, hollow, spherical, low density, free-flowing, alumino-silicate microspheres used as a versatile lightweight filler. The spheres are so tiny (as small as 5 microns) that the material appears to be a typical ceramic powder. For typical grades of Fillite 50-100% passes a 100 micron sieve.

Average Particle Density - 0.78 - 0.95 g/cc
Average Bulk Density - 0.4 - 0.49 g/cc (25-32 lbs/ft3)
Packing Factor - 60% - 65%
Hardness - Mohs Scale 5
Average Wall Thickness - 5 - 10% Sphere Diameter
Melting Temperature - 1200°-1350°C (2190°-2460°F)
Thermal Conductivity - 0.11 Wm- 1k-1
Loss on Ignition - 4% maximum
Surface Moisture - 0.3% maximum
Crush Strength - 1500 - 3000 psi
Oil Absorption - 16 - 18 g oil/100 g

Hebei Gator Chemicals Tech Co., Ltd. also produces Cenospheres. They list a similar chemistry but also show TiO2 at 0.5% - 1.5%.
Size: 20-200 Mesh


PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy