Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Hommel Frit 22

Description: Low Lead Frit Boron Frit

Oxide Analysis Formula Tolerance
CaO 6.83% 0.47
PbO 30.65% 0.53
B2O3 17.67% 0.98
SiO2 44.85% 2.88
Oxide Weight 386.00
Formula Weight 386.00

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.