1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Frit Fsb510/866

Description: High Alkaline Borosilicate Frit

Oxide Analysis Formula Tolerance
SiO2 45.00% 1.77
Al2O3 2.00% 0.05
B2O3 29.00% 0.98
Na2O 13.00% 0.50
CaO 12.00% 0.50
Oxide Weight 238.44
Formula Weight 238.44

Notes

One of the few frits available to potters in South Africa. An approximate chemistry but should be fairly close.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 1080C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy