PotteryCrafts Frit P2959

Alternate Names: PotteryCrafts Frit 2950

Description: Low Expansion Frit

Oxide Analysis Formula Tolerance
SiO2 65.84% 5.00
MgO 2.21% 0.25
Al2O3 6.71% 0.30
Na2O 5.44% 0.40
CaO 3.69% 0.30
B2O3 15.23% 1.00
ZnO 0.89% 0.05
Oxide Weight 456.06
Formula Weight 456.06

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs http://www.potterycrafts.co.uk/Products/0028000b
PotteryCrafts Frit information
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy