Frit 35.680

Alternate Names: Frit 35 680, Frit 35-680

Oxide Analysis Formula Tolerance
Na2O 5.08% 0.36
CaO 6.90% 0.53
PbO 5.72% 0.11
B2O3 12.48% 0.78
Al2O3 8.10% 0.34
SiO2 61.73% 4.45
Oxide Weight 433.77
Formula Weight 433.77

Related Information

Data

Frit Melting Range (C) 960-1080C