Alternate Names: 37 960,37-960
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 1.00% | 1.00 | |
| B2O3 | 1.09% | 0.63 | |
| Al2O3 | 0.32% | 0.13 | |
| SiO2 | 1.87% | 1.25 | |
| Oxide Weight | 172.48 | ||
| Formula Weight | 172.48 | ||
| Frit Melting Range (C) | 1000-1120C |
|---|