Frit 37.528

Alternate Names: Frit 37 528, Frit 37-528

Oxide Analysis Formula Tolerance
CaO 7.32% 0.50
Na2O 6.47% 0.40
MgO 0.53% 0.05
ZnO 1.06% 0.05
B2O3 14.34% 0.79
Al2O3 8.51% 0.32
SiO2 61.77% 3.94
Oxide Weight 383.13
Formula Weight 383.13

Related Information

Data

Frit Melting Range (C) 940-1060C