Description: Fritte au zinc
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 2.99% | 0.12 | |
| ZnO | 38.77% | 0.77 | |
| Na2O | 4.22% | 0.11 | |
| Al2O3 | 5.68% | 0.09 | |
| SiO2 | 40.15% | 1.08 | |
| B2O3 | 8.18% | 0.19 | |
| Oxide Weight | 161.65 | ||
| Formula Weight | 161.65 | ||
Corrected this chemistry Oct 2022, it was:
Na2O 4.0, ZnO 39.0, MgO .12, Al2O3 .095, SiO2 1.077
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| URLs |
http://www.casparceramique.ch/articles-1/frittes,41,g2-1-1-169-0.html
Frittes de Les Argiles du Moulin |
| Frit Softening Point | 590C |
|---|
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk